The current shuts off after some production time, or you receive cans with “stitching/glueing mode”

Cause:

The actual value of the weld power limiter increases with the heating of the machine.


Corretive:

Readjust the weld power limiter, to a higher value. Observe the “Max” value from a “cold “ start to a “warm up” machine during production. See also note below.


NOTE:

Power limit to activate the weld guard (stitch welding). Normally 5 – 10 % more than the actual “Max” value during production.
0 = Weld Power Limiter Off !

 